Polski

The influence of post-processing methods on the fatigue performance of materials prepared by selective laser melting

221
2025-01-17 14:28:07
Zobacz tłumaczenie

Researchers from Opole University of Technology in Poland have reported the latest progress in studying the effect of post-processing methods on the fatigue performance of materials prepared by selective laser melting (SLM). The related research was published in The International Journal of Advanced Manufacturing Technology under the title "Influence of post processing methods on fatigue performance of materials produced by selective laser melting (SLM)".

Although selective laser melting (SLM) can manufacture complex and customized products, the fatigue performance of parts manufactured by SLM is reduced compared to forged parts. The main factors causing this difference are the imperfect manufacturing parameters and inherent defects in the process itself. Even with the use of optimal manufacturing parameters, there is still variability in fatigue performance. However, it has been proven that using post-processing methods to reduce or eliminate defects is an effective way to improve fatigue performance.

This article provides a detailed introduction to various post-processing methods that can be used to modify surface and subsurface defects as well as internal defects. Each method demonstrates different potentials in generating beneficial residual compressive stress (CRS), altering surface and subsurface defects, and improving fatigue performance. The study found that considering the cyclic process, the impact of different post-processing methods varies. This article explores the conflicting research results that need further clarification. In addition, this article provides an in-depth review of the types and characteristics of defects that may affect fatigue performance, emphasizing the necessity of understanding these defects. The article points out the research gaps in existing post-processing methods and plans for future research directions, with a focus on technologies that have not been fully utilized but have potential for change.


Figure 1a Schematic diagram of components and process for selective laser melting (SLM); Possible internal and surface defects in SLM process.


Figure 2 Selective laser melting process parameters, key material characteristics, defects in SLM parts, and commonly used post-processing methods.


Figure 3a Schematic diagram of laser peening process and the resulting surface deformation; Laser scanning path and parameters.


Figure 4: The effect of laser peening on the performance of SLM parts; Measurement results of surface roughness and porosity before (a) and after (b) laser peening; Electron backscatter diffraction (EBSD) patterns of Ti64 treated with SLM before (c) and after (d) laser peening; Cross sectional views of AlSi7Mg in AB state (e) (a 'and b') and after laser peening (c ', d', e '); High magnification image of pores after laser peening (d '). The fracture surface of AlSi10Mg treated with SLM and post-treatment (f).


Figure 5 Shot peening process configuration and process parameters.


Figure 6: The effect of post-processing on surface and subsurface defects; (a) SLM fatigue specimen; (b) And (c) the surface roughness of unprocessed samples; (d) The sample treated with vibration light decoration failed due to crack nucleation at the surface and subsurface opening defects; (e) The crack initiation defect (√ area=98 µ m) that may cause material failure under cyclic loading.


Figure 7 SLM process parameters with defect types (a); Post processing methods and their effects on surface, subsurface, and internal defects (b); The impact of post-processing on defect resolution (c). C1, (MP) sample; Surface and subsurface pores of C2 and MP; C3,AB+SP; Uneven microstructure of C4 and SP; C5, HT specimens; The fracture morphology of C6 and HT samples; C7, Samples treated with hot isostatic pressing (HIP); C8, porosity before and after HIP treatment.


This article comprehensively reviews the relevant research on the influence of post-processing methods on the fatigue performance of selective laser melting (SLM) parts. Research has found that surface and subsurface defects, internal defects, microstructure, residual stress, and surface roughness are important factors affecting the fatigue performance of SLM parts. Laser peening has shown its potential in closing subsurface pores and generating deeper residual compressive stresses (CRS) than shot peening, although this can increase surface roughness.
However, shot peening can improve residual stress and surface roughness while forming a thicker residual compressive stress layer. The high roughness and uneven residual stress distribution generated during laser peening can lead to a decrease in fatigue performance. However, using continuous shot peening can improve fatigue performance without negatively affecting surface roughness. By creating good surface characteristics, mechanical processing has the ability to manufacture SLM parts with longer fatigue life.

However, this method has limitations in altering the transverse residual stress (TRS) and anisotropic behavior inside printed parts. Although heat treatment methods cannot improve surface properties, they can effectively change this harmful stress, but this method can lead to an increase in pores. Although hot isostatic pressing (HIP) cannot enhance surface properties, it has been proven to alter microstructure, refine anisotropy, close internal pores, and increase overall material density, thereby extending fatigue life.

The combination of hot isostatic pressing and mechanical processing, followed by polishing treatment, has been proven to produce SLM parts with superior fatigue performance even compared to traditional manufacturing parts. Not all defects affect the fatigue life of materials, but defects near the surface and large-sized internal defects (LOFs) with sharp edges are the main defects that lead to a decrease in material durability.

This article focuses on introducing post-processing methods that have not been widely studied and proposes future research directions. By evaluating the commonly used post-processing techniques in SLM, this article provides insightful guidance for improving the reliability of industries such as aerospace, energy, automotive, and biomedical implants in high stress applications.

Source: Yangtze River Delta Laser Alliance

Powiązane rekomendacje
  • Assisting Gas Mixing to Promote the Development of Fiber Laser Technology

    Just ten years ago, fiber laser cutting machines were considered experts in thin plates. The stores quickly realized that they had to invest in them to compete, at least by reducing their instrument materials. For high-quality sheet metal cutting, CO2 laser is still the way to go. Of course, fiber lasers can cut thicker blanks, but the quality is not very good, and their speed advantage almost dis...

    2024-01-11
    Zobacz tłumaczenie
  • Scientists have made breakthrough progress in using laser to cool sound waves

    A group of researchers from the Max Planck Institute of Optoelectronics has made a significant breakthrough in using laser cooling to travel sound waves. This development brings us one step closer to the quantum ground state of sound in waveguides, which is of great significance for quantum communication systems and future quantum technology.By using laser cooling, scientists can significantly red...

    2024-01-22
    Zobacz tłumaczenie
  • A new approach to 3D printing has been published in a Nature journal

    In the last century, the improvement of mechanical properties of structural metals was mainly achieved through the creation of increasingly complex chemical compositions. The complexity of this ingredient increases costs, creates supply fragility, and makes recycling more complex.As a relatively new metal processing technology, metal 3D printing provides the possibility to re-examine and simplify ...

    2024-11-29
    Zobacz tłumaczenie
  • Acousto optic modulation of gigawatt level laser pulses in the ambient air of Nature Photonics

    An interdisciplinary research group, including the German synchrotron radiation accelerator DESY and the Helmholtz Institute in Jena, Germany, reported that invisible gratings made of air not only are not damaged by lasers, but also maintain the original quality of the beam. The relevant research has been published in Nature Photonics under the title of "Acousto opt modulation of gigawatt scale la...

    2023-10-12
    Zobacz tłumaczenie
  • CO2 laser cutting machine for battery shell shaped parts: an innovative tool in energy technology manufacturing

    The development of new energy technology has made battery technology the engine for advancing clean energy. In battery manufacturing, the cutting of battery shell shaped parts is a crucial step. CO2 laser cutting machines have become an innovative tool for promoting the development of this field due to their high efficiency and precision. This article will delve into the important characteristics ...

    2023-12-25
    Zobacz tłumaczenie