Русский

Overview of Inconel 939 Alloy Parts Developed by Additive Manufacturing Process

210
2024-12-10 12:00:28
Посмотреть перевод

The related paper was published in Heliyon under the title "A systematic review of Inconel 939 alloy parts development via additive manufacturing process".

IN939 is a modern nickel based high-temperature alloy that can work continuously at high temperatures due to its excellent fatigue resistance, creep resistance, and corrosion resistance. The unique performance of IN939 is related to the composition of the alloy and specific post-treatment processes (such as solution treatment and aging treatment), resulting in features such as γ 'residues and MC and M23C6 carbides. This also includes the lack of eutectic and primary melting phases. For this alloy, the main component development is carried out through the powder bed melting process using a laser powder bed melting machine. Meanwhile, a separate study emphasized the synthesis of EB-PBF devices. The additive manufacturing process of these alloys is hindered by machine parameters, which have been found to be unable to obtain fully dense structures with the required properties alone. The purpose of these parameters is to improve its core performance while minimizing defects related to powder metallurgy processes, such as porosity, harmful precipitation, grain anisotropy, etc. This study aims to provide an overview of research progress related to IN939, with a clear focus on benchmarks achieved through additive manufacturing technology. Researchers discussed the work done in this field, compared the results of different studies, and identified gaps in current research. Through these works, researchers aim to gain a comprehensive understanding of the potential of IN939 and its applications in extreme environments.



Figure 1. Main aspects of developing IN939 components.

 


Figure 2. Microstructure of the casting sample.


Figure 3. Microstructure of the sample annealed at 1100 ℃ for 4 hours and then water quenched.


Figure 4. Main categories and software usage of additive manufacturing.


Figure 5. Simple schematic diagram of selective laser melting process for metal/alloy parts.


Figure 6. Schematic diagram of electron beam melting process.


Figure 7. Schematic diagram of direct energy deposition through (a) powder material feeding and (b) metal wire material feeding.


Figure 8. Schematic diagram of metal adhesive spraying process.


Figure 9. Fracture surfaces of (a) undisturbed specimen, (b) LTH specimen, (c) HTH specimen, and (d) cast LTH specimen subjected to creep rupture at 816 ℃/250 MPa.


Figure 10. Optical image of partially recast layer of the sample.


Figure 11. Scanning electron microscopy images of SLM samples (a, b) after aging without solution treatment, (c) after solution treatment+aging.


Figure 12. a, b) Cut the pit thickness and recast area of the sample. (c) Optical microscope images of the recast layer and HAZ area of CFG and (d) wire EDM methods.


Figure 13. Scanning electron microscopy microstructure images of the sample at different heights (b, c) 40mm, (d, e) 30mm, (f, g) 20mm, and (h, i) 10mm along the molding direction.


Inconel 939 additive manufacturing has been explored for advanced applications, which has led to further exploration of the impact of components and process parameters on this age hardening alloy. However, finished IN939 samples typically exhibit residual thermal strain, stress, and porosity, which may have a negative impact on their performance. To address these challenges, post-processing is considered crucial in achieving sample homogenization, controlling its microstructure, and reducing porosity. Although these processing methods have many benefits, they often require multiple steps and complex loops to form the required stages. These advances in AM and post-processing technology are expected to broaden the application range of IN939 parts and improve their performance in extreme environments. However, in addition to optimizing the microstructure and mechanical properties of IN939 parts, the performance of IN939 parts still needs to be further improved. Researchers can develop more targeted methods to optimize the performance of IN939 components and expand their potential applications by understanding their behavior in extreme environments rather than current developments. Combining hot isostatic pressing with optimized parameters at different stages of the multi-step heat treatment process can result in components with uniform microstructure and excellent isotropic mechanical properties.

Source: Yangtze River Delta Laser Alliance

Связанные рекомендации
  • Accurate measurement of neptunium ionization potential using new laser technology

    Neptunium is the main radioactive component of nuclear waste, with a complex atomic structure that can be explored through mass spectrometry. This analysis is crucial for understanding its inherent characteristics and determining the isotopic composition of neptunium waste. Magdalena Kaja and her team from Johannes Gutenberg University in Mainz, Germany have developed a novel laser spectroscopy te...

    2024-05-11
    Посмотреть перевод
  • Observation of laser power changes in ultrafast protein dynamics

    When researchers at the Max Planck Institute of Medicine conducted their first ultrafast X-ray crystallographic experiment on myoglobin in 2015, they were not aware that they had conducted the wrong experiment. By increasing the power of X-ray free electron lasers to ensure usable diffraction patterns, lead researcher Ilme Schlichting said that they "suddenly entered the wrong [excited] state with...

    2024-02-28
    Посмотреть перевод
  • Fujitsu collaborates to research and develop multi band wavelength fiber optic transmission technology

    Recently, Fujitsu and KDDI research company have successfully developed a high-capacity multi band wavelength multiplexing transmission technology using installed optical fibers.The new technology of the two companies can transmit wavelengths beyond the C-band by using batch wavelength conversion and multi band amplification technology.Expanding transmission capacity in remote areasTwo companies h...

    2023-12-05
    Посмотреть перевод
  • More penetrating than X-rays μ Meson imaging is expected to be advanced with high-power lasers

    μ Mesons are naturally occurring subatomic particles that can penetrate much deeper dense matter than X-rays. Therefore, μ Meson imaging can enable scientists to capture images of nuclear reactors, volcanoes, tsunamis, and hurricanes. However, this process is slow, as it occurs naturally μ The low flux of mesons requires several months of exposure time for the image.It is understood that ...

    2023-11-01
    Посмотреть перевод
  • Significant progress has been made in the research on the detection of microwave electric fields in the Rydberg area of Shanghai Institute of Optics and Technology

    Recently, the Aerospace Laser Technology and System Department of the Shanghai Institute of Optics and Precision Mechanics, Chinese Academy of Sciences, and the East China Research Team of the Key Laboratory of Quantum Optics, Chinese Academy of Sciences, together with the research team of Professor Chen Liqing of East China Normal University, demonstrated a Rydberg microwave sensor with high sens...

    2024-05-08
    Посмотреть перевод