Defects and solutions that are prone to occur when laser welding square shell battery explosion-proof valves for power batteries

488
2023-09-15 14:27:20
Δείτε τη μετάφραση

For example, the commonly used square shell battery cells for power batteries include laser welding of cover explosion-proof valves, laser welding of pole columns, and laser welding of cover plates and shells. During the process of laser welding of aluminum alloy, it is easy to generate unqualified phenomena such as explosion points, pores, welding cracks, excessive depth and width of fusion. 

Therefore, it is necessary to define the impact of unqualified items, analyze the consequences (degree of harm) of the impact, understand the mechanism of laser welding unqualified, and take effective measures to improve the quality and consistency of laser welding in the mass production stage, improve the output of the production line, and reduce welding unqualified, Reduce the cost of waste materials.

Common failures in sealing welding of battery explosion-proof valves
Explosion proof valve is a circular thin sheet of pure aluminum (1060 or 3003) with a thickness between 0.08 and 0.1 mm. When using infrared fiber laser welding, due to the high reflectivity of solid aluminum material towards infrared laser and its thin material, if the welding process is not appropriate, the explosion-proof valve is prone to overheating, perforation or explosion during the laser welding process, causing it to lose its pressure relief and explosion-proof function.

Potential failure 1: Over burning/melting through
Reason: When using infrared laser welding, due to the high reflectivity of the solid aluminum alloy surface to infrared laser, higher laser power is often used. However, the thickness of the explosion-proof valve from 0.08 to 0.1 mm is too small, making it easy to melt through.
Solution suggestion: Select appropriate welding process parameters to achieve a steep increase and slow decrease in laser power and control heat input. Adopting a waveform with a pre peak and exponential attenuation can improve the absorption rate of aluminum material to laser, while the subsequent exponential attenuation wave can prevent perforation caused by high power density.

Potential Failure 2: Burst Hole
Cause: Gas escape from the molten pool during laser welding.
Source of gas:
1. The power battery cover plate and explosion-proof valve are thin stamping parts that are prone to residual lubricating oil and cleaning fluid after processing. Under the action of high-power density laser, these liquids are easily vaporized and float up to the surface of the molten pool, causing a large amount of splashing and leaving pits on the surface of the weld, forming explosive holes.

2. The width to thickness ratio of explosion-proof valves can generally reach around 30, and during welding, it is easy to cause thermal deformation and warping due to heating, resulting in a large amount of air in the assembly gap between the explosion-proof valve and the top cover. During welding, these residual air expands and sprays out the molten pool, forming explosive holes.

Suggested solution: 
1. Thoroughly clean the cover plate and explosion-proof valve before welding; 
2) Optimize the welding process by using pre spot welding and seam welding, and prevent warping and deformation through spot welding fixation to reduce blast hole defects.

In the laser welding of power square shell batteries, welding process technicians will select appropriate laser and welding process parameters based on the customer's battery material, shape, thickness, tensile requirements, etc., including welding speed, waveform, peak value, welding head tilt angle, etc. to set reasonable welding process parameters to ensure that the final welding effect meets the requirements of the power battery manufacturer.

Source: Shangtuo Laser

Σχετικές προτάσεις
  • Siemens will provide Rolls Royce with aerospace additive manufacturing components

    Recently, Siemens Energy's Materials Solutions division (hereinafter referred to as Siemens) officially signed a cooperation agreement with Rolls Royce, a well-known enterprise in the field of aviation engines in the UK, agreeing that Siemens will develop and supply mass-produced additive manufacturing components for Rolls Royce's civil aerospace business.Rolls Royce and 3D Printing TechnologyRoll...

    2024-12-13
    Δείτε τη μετάφραση
  • German team develops and promotes laser technology for formable hybrid components

    Scientists from the Hanover Laser Center (LZH) in Germany are studying two laser based processes for producing load adapted hybrid solid components.From a transaction perspective, mixing semi-finished products can help save materials and production costs, but if the components that need to be replaced are made of expensive materials, these materials need to meet high requirements in future use, su...

    2023-08-16
    Δείτε τη μετάφραση
  • The researchers expect the EUV lithography market to grow from $9.4 billion in 2023 to $25.3 billion in 2028

    The researchers estimate the period from 2023 to 2028. EUV lithography will address the limitations of traditional optical lithography, which has reached its physical limits in terms of resolution. The shorter wavelength of EUV light allows for the creation of smaller features and tighter patterns on silicon wafers, enabling the manufacture of advanced microchips with greater transistor densities....

    2023-08-04
    Δείτε τη μετάφραση
  • Edmund Optics acquisition son-x

    Recently, globally renowned optical component manufacturer Edmund Optics announced that the company has acquired ultrasonic assisted systems and high-precision optical manufacturer son-x.Edmund Optics, as a leader in optical technology solutions, has been serving various fields such as life sciences, biomedicine, industrial testing, semiconductors, and laser processing since its establishment in 1...

    01-22
    Δείτε τη μετάφραση
  • Application of Multipurpose Femtosecond Laser Interferometry in High Precision Silicon Nanostructures

    Researchers from the Laser Processing Group of the IO-CSIC Institute of Optics in Spain report on the application of multi-purpose femtosecond laser interference in high-precision silicon nanostructures. The related research was published in Optics&Laser Technology with the title "Versatile femtosecond laser interference pattern applied to high precision nanostructured of silicon".Highlights:...

    2024-07-10
    Δείτε τη μετάφραση